“2. PSP (Primary Surface Preparation)
2.1 Blasting and profile6, 7
Sa 2 1/2; with profiles between 30-75 μm
Blasting shall not be carried out when:
.1 the relative humidity is above 85%; or
.2 the surface temperature of steel is less than 3°C above the dew point."