Thickness measurement requirements
|
1. Within the cargo area
- .1 Each deck plate
- .2 Three transverse sections
- .3 Each bottom plate
|
2.
Measurements of structural members subject to close-up survey according to
table above (for close up survey), for general assessment and recording of
corrosion pattern
|
3. Suspect
areas
|
4. Selected
wind and water strakes outside the cargo area
|
5. All wind
and water strakes outside the cargo area
|
6. Internal
structure in the fore and aft peak tanks
|
7. All
exposed main deck tanks outside the cargo area and all exposed first tier
superstructure deck plates
|
Guidance
notes:
|
1 The attending surveyor(s) may increase the
extent of thickness measurements as deemed necessary (see paragraph 7.3.5 of the CAS).
|
2 Transverse sections for thickness measurements
shall be chosen where the largest material reductions are expected to occur
or are revealed from deck plating measurements (see section 7.3.8 of the CAS).
|
3 Where substantial corrosion is found, the extent
of thickness measurements shall be increased accordingly (see paragraph
7.3.4 of the CAS).
|